Home / Guide / Injection Molding Defects Guide

Injection Molding Defects — Complete Guide to Causes, Solutions & Prevention

Injection molding defects are unavoidable in production, but understanding their root causes allows molders to minimize scrap rates and maintain consistent quality. This guide covers the most common injection molding defects — their causes, solutions, and how to prevent them through proper mold design and process parameter optimization.

1. Warpage

Description: Warpage occurs when different areas of a molded part shrink at different rates, causing the part to distort, bend, or twist out of its intended shape. It is one of the most challenging defects to resolve because it often requires both mold design changes and process adjustments.

Causes:

Solutions:

2. Sink Marks

Description: Sink marks appear as local depressions or dimples on the surface of a molded part, typically opposite thick wall sections, ribs, or bosses. They occur when the outer surface solidifies first and the inner material shrinks as it cools, pulling the surface inward.

Causes:

Solutions:

3. Flash

Description: Flash is a thin layer of plastic that escapes from the mold cavity along the parting line, around ejector pins, or through venting channels. It creates a burr-like excess material that requires secondary trimming.

Causes:

Solutions:

4. Weld Lines (Knit Lines)

Description: Weld lines form where two or more flow fronts meet inside the mold cavity. The meeting point may not fully bond, creating a visible line that is often weaker than the surrounding material.

Causes:

Solutions:

5. Short Shots

Description: A short shot occurs when the mold cavity is not completely filled, leaving an incomplete part. This is one of the most obvious defects and is typically caught during first-shot validation.

Causes:

Solutions:

6. Burn Marks

Description: Burn marks appear as black or brown discolored areas on the molded part, usually at the end of fill or in dead-end areas where trapped air is compressed and ignited.

Causes:

Solutions:

7. Flow Lines

Description: Flow lines are wavy, ring-shaped, or streaked surface patterns that appear on the molded part. They are caused by the molten plastic solidifying in waves as it advances through the cavity.

Causes:

Solutions:

8. Jetting

Description: Jetting occurs when molten plastic shoots through a gate or narrow restriction and snakes into an open cavity without contacting the mold walls, creating a serpentine pattern on the part surface.

Causes:

Solutions:

Defect Prevention Through Mold Design

Many injection molding defects can be prevented at the design stage. Key DFM (Design for Manufacturing) principles include:

Process Troubleshooting Quick Reference

Problem Primary parameter to adjust Secondary check
Short shot Increase shot size Check nozzle for blockage
Flash Increase clamping force Inspect parting surface
Sink marks Increase hold pressure/time Check wall thickness
Warpage Balance cooling Adjust mold temperature zones
Weld lines Increase melt temperature Check gate location
Burn marks Improve venting Reduce injection speed
Flow lines Increase injection speed Raise mold temperature
Jetting Reduce injection speed (first stage) Check gate location/type
Blisters Dry material Reduce melt temperature
Splay/Silver streaks Dry material thoroughly Reduce excessive shear

Why Material Drying Matters

Many injection molding defects — including splay (silver streaks), blisters, and brittleness — are caused by moisture in the plastic material. Hygroscopic materials like nylon (PA), polycarbonate (PC), and ABS absorb moisture from the atmosphere and must be dried before processing.

Material Drying temperature Drying time Max moisture content
PA6 (Nylon 6) 80°C 4-6 hours < 0.2%
PC (Polycarbonate) 120°C 3-4 hours < 0.02%
ABS 80-85°C 2-4 hours < 0.1%
PBT 120°C 3-6 hours < 0.05%
PMMA (Acrylic) 80-85°C 2-4 hours < 0.05%

Partnering with MFGABC

At MFGABC, our engineers conduct a comprehensive DFM (Design for Manufacturing) analysis before any tool is cut. We identify potential defect risks — such as weld line locations, filling imbalances, or cooling issues — and adjust the mold design before steel is cut. This proactive approach significantly reduces trial-and-error during mold commissioning.